Oxford 80 Plus RIE
Revision as of 13:26, 29 April 2022 by Dsbarth (talk | contribs) (Protected "Oxford 80 Plus RIE" ([Edit=Allow only administrators] (indefinite) [Move=Allow only administrators] (indefinite)) [cascading])
| Tool Name | Oxford 80 Plus RIE |
|---|---|
| Instrument Type | Etch |
| Staff Manager | Sam Azadi |
| Lab Location | Bay 2 |
| Tool Manufacturer | Oxford Instruments |
| Tool Model | 80+ |
| NEMO Designation | {{{NEMO_Designation}}} |
| Nearest Phone | 215-898-9748 |
| SOP Link | QNF SOP |
Description
Oxford 80 Plus is an anisotropic dry etch tool. The main use of this tool is to etch SiO2, and SiNx to create hard masks for deep Si etch. However, it etches many other materials, including a variety of resists. The tool is connected to the following gases: Ar, O2, CF4, CHF3, SF6.
The plasma is ignited by the oscillating electric field created by the RF power at 13.56 MHz. The wafer is cooled down via passive cooling through a graphite chuck.
Applications
- Etch of SiO2
- Etch of SiNx
- Etch of Si
- Etch of resist
Resources
SOPs & Troubleshooting