Heidelberg DWL 66+ Laser Writer

From Quattrone Nanofabrication Facility
Revision as of 15:55, 23 December 2022 by Davijon (talk | contribs)
Jump to navigation Jump to search


Heidelberg DWL 66+ Laser Writer
LW-01.jpeg
Tool Name Heidelberg DWL 66+ Laser Writer
Instrument Type Lithography
Staff Manager David Jones
Lab Location Bay 2
Tool Manufacturer Heidelberg
Tool Model DWL 66+
NEMO Designation {{{NEMO_Designation}}}
Nearest Phone 8-9799
SOP Link SOP

Description

The fully automated DWL 66+ laser writing system is located inside an environment chamber for stable environment of the system with controlled laminar airflow and temperature stability. The chamber is situated on a granite base with air cushions for vibration isolation. The optical system includes highly reflective mirrors and acousto-optic modulators for real-time beam correction.

Lens & Resolution

  • 2 mm lens (optical autofocus): 600 nm
  • 10 mm lens (pneumatic autofocus): 2 µm
  • 40 mm lens (pneumatic autofocus): 10 µm


Applications
  • Patterning of photomasks
  • Direct laser writing of patterns

Processes

The following exposure parameters may be used to direct write into S1800 resist (soft baked at 115C for 1 minute) with the 10mm write head. For the optimum focus, please refer to the "AZ1500.txt" or "IP3500.txt" files for the optimum value to use.


Resources

SOPs & Troubleshooting