The QNF provides a variety of standard resists to meet demands for most applications. Some specialty resists are also sold through the QNF Stockroom. A summary of stocked resists along with some processing information can be found in the table below. Other similar options that may be available in QNF are also listed.
QNF Supplied Standard Photoresists
| Resist |
Tone |
Notes |
Alternatives |
Datasheet
|
| S1805 |
+ |
General |
KL5305 |
Datasheet
|
| S1813 |
+ |
General |
KL5315 |
Datasheet
|
| S1818 |
+ |
General |
|
Datasheet
|
| SPR 220-3 |
+ |
Etch |
KPRO-3, KL6003, AZ3330F |
Datasheet
|
| SPR 220-4.5 |
+ |
Etch |
KPRO-3, KL6003, AZ3330F |
Datasheet
|
| SPR 220-7 |
+ |
Etch |
AZ 12XT, AZ P4620 |
Datasheet
|
| AZ 3330F |
+ |
General, Metal RIE, Plating |
SPR 220-3, SPR 220-4.5, K-PRO 3, KL6003 |
Datasheet
|
| NR7-3000P |
- |
Etch, General |
|
Datasheet
|
| APOL-LO 3202 |
- |
Liftoff |
|
Datasheet
|
| IP-Dip |
- |
Nanoscribe |
|
|
| HARE SQ 2 |
- |
Epoxy |
SU-8 2005 |
Datasheet
|
| HARE SQ 50 |
- |
Epoxy |
SU-8 2050 |
Datasheet
|
Stockroom Photoresists
| Resist |
Tone |
Notes |
Alternatives |
Datasheet
|
| SU-8 2005 |
- |
Epoxy |
HARE SQ 2 |
Datasheet
|
| SU-8 2050 |
- |
Epoxy |
HARE SQ 50 |
Datasheet
|
| SU-8 2100 |
- |
Epoxy |
HARE SQ 50 |
Datasheet
|
| SU-8 3050 |
- |
Epoxy |
HARE SQ 50 |
Datasheet
|