Difference between revisions of "IPG IX280-DXF Green Micromachining Laser"
Jump to navigation
Jump to search
(Created page with "Category:Back End {{EquipmentInfo | name = IPG IX280-DXF Green Micromachining Laser | Tool_Name = IPG IX280-DXF Green Micromachining Laser | image = Image:LMM-02.jpeg|3...") |
|||
| Line 7: | Line 7: | ||
| imagecaption = | | imagecaption = | ||
| Instrument_Type = Back End | | Instrument_Type = Back End | ||
| − | | Staff_Manager = | + | | Staff_Manager = Eric Johnston |
| Lab_Location = Bay 2 | | Lab_Location = Bay 2 | ||
| Tool_Manufacturer = IPG | | Tool_Manufacturer = IPG | ||
Revision as of 08:52, 30 March 2022
| Tool Name | IPG IX280-DXF Green Micromachining Laser |
|---|---|
| Instrument Type | Back End |
| Staff Manager | Eric Johnston |
| Lab Location | Bay 2 |
| Tool Manufacturer | IPG |
| Tool Model | IX280 |
| NEMO Designation | {{{NEMO_Designation}}} |
| Nearest Phone | 3-9639 |
| SOP Link | SOP |
Description
The IX280-DXF is a highly flexible laser micro-machining system for multipurpose, R&D and production applications. The system combines a Class 1 workstation integrated with a fiber laser and all necessary software.
Specifications
- Lasers at 532 or 1064 nm
- Pulse Energy up to 15 Joules (1064 nm)
- X-Y Positional Accuracy: <3 μm
- Z-theta Accuracy: <10 μm, ±0.02°
- Galvanometer Scanner or Fixed Optics
- Thermal Cutting Head
- Step and Scan Stage/ Galvo Integration
- Vision System Resolution 0.12 μm/ pixel
- DXF and CSV File Interface
Applications
Cutting Applications
- Ceramics, Metals, Polymers and Semiconductor Materials
- Patterning of ITO and other Thin-films
Drilling Applications
- Hole Diameters down to 15 μm