{| class="wikitable" style="vertical-align:bottom;"
 
{| class="wikitable" style="vertical-align:bottom;"
 
|-
 
|-
 +
!
 +
! mW/cm^2
 +
! % of output
 +
|-
 
| NO MASK
 
| NO MASK
| ~10 mW/cm^2
+
| ~10  
| 100% of output
+
| 100%
 
|-
 
|-
 
| GLASS MASK
 
| GLASS MASK
| ~9 mW/cm^2
+
| ~9
 
| 87.5%
 
| 87.5%
 
|-
 
|-
 
| GLASS + FILM MASK
 
| GLASS + FILM MASK
| ~7 mW/cm^2
+
| ~7
 
| 68.5%
 
| 68.5%
 
|-
 
|-
 
| GLASS + LP FILTER  
 
| GLASS + LP FILTER  
| ~5 mW/cm^2
+
| ~5
| 47.0%
+
| 47%
 
|-
 
|-
 
| GLASS + FILM + LP FILTER  
 
| GLASS + FILM + LP FILTER  
| ~4 mW/cm^2
+
| ~4
| 37.0%
+
| 37%
 
|}
 
|}
  

Latest revision as of 11:52, 29 April 2025


ABM Mask Aligner
Tool Name ABM Mask Aligner
Instrument Type Lithography
Staff Manager Ana Cohen
Lab Location Bay 6
Tool Manufacturer ABM
Tool Model
NEMO Designation MA-03
Lab Phone xxxxx
SOP Link SOP

Description

The ABM Mask Aligner is a manual and versatile mask aligner with top-side alignment and substrate capabilities from 100mm down to small pieces. Requires a 5" mask or 5" glass plate with film mask.

Applications

Tool is used primarily for SU8 exposure. It can also be used for aligning PDMS components for PDMS-to-PDMS bonding.

Exposure time = dose (mJ/cm^2) / intensity (mW/cm^2) Dose can be determined from the resist data sheet. See table below for intensities.

To obtain vertical sidewalls with a Cr glass mask, use the long pass filter (PL-360-LP) which eliminates UV emission below 350nm. Do not use with film masks. Inherent defects in film masks will be accentuated, resulting in worse results.

mW/cm^2 % of output
NO MASK ~10 100%
GLASS MASK ~9 87.5%
GLASS + FILM MASK ~7 68.5%
GLASS + LP FILTER ~5 47%
GLASS + FILM + LP FILTER ~4 37%

More information about Soft Lithography processing can be found under Process Resources