Difference between revisions of "Resists at QNF"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
(Created page with "The QNF provides a variety of standard resists to meet demands for most applications. Some specialty resists are also sold through the QNF Stockroom. A summary of stocked resi...")
 
Line 1: Line 1:
 
The QNF provides a variety of standard resists to meet demands for most applications. Some specialty resists are also sold through the QNF Stockroom. A summary of stocked resists along with some processing information can be found in the table below. Other similar options that may be available in QNF are also listed.
 
The QNF provides a variety of standard resists to meet demands for most applications. Some specialty resists are also sold through the QNF Stockroom. A summary of stocked resists along with some processing information can be found in the table below. Other similar options that may be available in QNF are also listed.
  
== QNF Supplied Standard Photoresists ==
+
=== QNF Supplied Standard Photoresists ===
 
{| class="wikitable sortable"
 
{| class="wikitable sortable"
 
! Resist !! Tone !! Notes !! Alternatives !! Datasheet
 
! Resist !! Tone !! Notes !! Alternatives !! Datasheet

Revision as of 13:55, 10 May 2023

The QNF provides a variety of standard resists to meet demands for most applications. Some specialty resists are also sold through the QNF Stockroom. A summary of stocked resists along with some processing information can be found in the table below. Other similar options that may be available in QNF are also listed.

QNF Supplied Standard Photoresists

Resist Tone Notes Alternatives Datasheet
S1805 + General KL5305 Datasheet
S1813 + General KL5315 Datasheet
S1818 + General Datasheet
SPR 220-3 + Etch KPRO-3, KL6003, AZ3330F Datasheet
SPR 220-4.5 + Etch KPRO-3, KL6003, AZ3330F Datasheet
SPR 220-7 + Etch AZ 12XT, AZ P4620 Datasheet
AZ 3330F + General, Metal RIE, Plating SPR 220-3, SPR 220-4.5, K-PRO 3, KL60003 Datasheet
NR7-3000P - Etch, General Datasheet
APOL-LO 3202 - Liftoff Datasheet
IP-Dip - Nanoscribe
HARE SQ 2 - Epoxy SU-8 2005 Datasheet
HARE SQ 50 - Epoxy SU-8 2050 Datasheet