== Description ==
 
== Description ==
Savannah is equipped with high-speed pneumatic pulse valves to enable our unique Exposure Mode™ for thin film deposition on Ultra High Aspect Ratio substrates. This proven precision thin film coating methodology can be used to deposit conformal, uniform films on substrates with aspect ratios of greater than > 2000:1.
+
The QNF Savannah ALD is equipped with high-speed pneumatic pulse valves to enable our unique Exposure Mode™ for thin film deposition on ultra high aspect ratio substrates. This proven precision thin film coating methodology can be used to deposit conformal, uniform films on substrates with aspect ratios of greater than > 2000:1.
  
The QNF Savannah is capable of holding substrates of different sizes (up to 200mm). It is equipped with six precursor lines for deposition of Al2O3, HfO2, TiO2, and SiO2.
+
The QNF Savannah ALD is capable of holding substrates of different sizes (up to 200mm). The system is equipped with six precursor lines for deposition of Al2O3, HfO2, TiO2, and SiO2.

Revision as of 11:55, 14 March 2022

Cambridge Nanotech S200 ALD
ALD-01.jpeg
Tool Name Cambridge Nanotech S200 ALD
Instrument Type Deposition
Staff Manager Sam Azadi
Lab Location Bay 2
Tool Manufacturer Ultratech/Cambridge
Tool Model S200
NEMO Designation {{{NEMO_Designation}}}
Nearest Phone XXXXX
SOP Link SOP

Description

The QNF Savannah ALD is equipped with high-speed pneumatic pulse valves to enable our unique Exposure Mode™ for thin film deposition on ultra high aspect ratio substrates. This proven precision thin film coating methodology can be used to deposit conformal, uniform films on substrates with aspect ratios of greater than > 2000:1.

The QNF Savannah ALD is capable of holding substrates of different sizes (up to 200mm). The system is equipped with six precursor lines for deposition of Al2O3, HfO2, TiO2, and SiO2.