Difference between revisions of "Oxford 80 Plus RIE"
Jump to navigation
Jump to search
m (Changed protection level for "Oxford 80 Plus RIE" ([Edit=Allow only autoconfirmed users] (indefinite) [Move=Allow only autoconfirmed users] (indefinite))) |
|||
| Line 34: | Line 34: | ||
===== SOPs & Troubleshooting ===== | ===== SOPs & Troubleshooting ===== | ||
* [https://repository.upenn.edu/scn_sop/7/ QNF SOP] | * [https://repository.upenn.edu/scn_sop/7/ QNF SOP] | ||
| + | |||
| + | * [https://upenn.box.com/s/slifsykn8u1s3rxnkabjxjjgp3pi9k8u ATPACT Manual] | ||
| + | |||
| + | * [https://upenn.box.com/s/luhzy81vv31ou9nh4cxwutz93b0pdrnf E 200T-600T Counters Manual] | ||
Revision as of 14:22, 30 August 2022
| Tool Name | Oxford 80 Plus RIE |
|---|---|
| Instrument Type | Etch |
| Staff Manager | Sam Azadi |
| Lab Location | Bay 2 |
| Tool Manufacturer | Oxford Instruments |
| Tool Model | 80+ |
| NEMO Designation | {{{NEMO_Designation}}} |
| Nearest Phone | 215-898-9748 |
| SOP Link | QNF SOP |
Description
Oxford 80 Plus is an anisotropic dry etch tool. The main use of this tool is to etch SiO2, and SiNx to create hard masks for deep Si etch. However, it etches many other materials, including a variety of resists. The tool is connected to the following gases: Ar, O2, CF4, CHF3, SF6.
The plasma is ignited by the oscillating electric field created by the RF power at 13.56 MHz. The wafer is cooled down via passive cooling through a graphite chuck.
Applications
- Etch of SiO2
- Etch of SiNx
- Etch of Si
- Etch of resist
Resources
SOPs & Troubleshooting