Difference between revisions of "SPTS Si DRIE"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
Line 30: Line 30:
 
== Resources ==
 
== Resources ==
 
[https://www.youtube.com/watch?v=UmRFj_2kdJ8 Training Part 1, Introduction & Wafer Cleaning]
 
[https://www.youtube.com/watch?v=UmRFj_2kdJ8 Training Part 1, Introduction & Wafer Cleaning]
 +
 
[https://www.youtube.com/watch?v=8zW80SfvrTM Training Part 2, Operating The Tool]
 
[https://www.youtube.com/watch?v=8zW80SfvrTM Training Part 2, Operating The Tool]
  
 
===== SOPs & Troubleshooting =====
 
===== SOPs & Troubleshooting =====
 
* [https://repository.upenn.edu/scn_sop/11 QNF SOP]
 
* [https://repository.upenn.edu/scn_sop/11 QNF SOP]

Revision as of 12:47, 29 March 2022


SPTS Si DRIE
DE-03.jpeg
Tool Name SPTS Si DRIE
Instrument Type Etch
Staff Manager Sam Azadi
Lab Location Bay 2
Tool Manufacturer SPTS
Tool Model Rapier
NEMO Designation {{{NEMO_Designation}}}
Nearest Phone XXXXX
SOP Link SOP

Description

SPTS Rapier is an anisotropic dry etch tool. The tool uses Bosch Process to etch silicon with high selectivity and nearly vertical sidewalls. Bosch process consists of two steps: 1) Deposition of a passivation layer, using C4F8 gas. This passivation layer is a polymer that protects the sidewalls from being etched. 2) A nearly vertical plasma etch step using SF6. A bias is applied in the chamber that forces the ions to attack the surface vertically and etch through the passivation layer at the bottom of the trench, exposing the silicon underneath. That Si is then etched within the same step. The passivation layer is also deposited inside the chamber and the etch results in a layer of deposited polymer inside the chamber walls which makes it critical to run a cleaning recipe at the end of each etch run.

Shorter cycle times result in smoother sidewalls while longer cycle times achieve higher etch rate. The tool in QNF is connected to Ar, O2,N2, C4F8, and SF6 gases.

Applications
  • Deep etching of Si