== Goal == | == Goal == | ||
| + | Determine the a-Si deposition rate on CVD-01 | ||
| − | |||
== Materials == | == Materials == | ||
| − | * SiO<sub>2</sub> | + | * 250 nm SiO<sub>2</sub> on Si. |
== Equipment == | == Equipment == | ||
Latest revision as of 13:54, 14 October 2024
Goal
Determine the a-Si deposition rate on CVD-01
Materials
- 250 nm SiO2 on Si.