{| class="wikitable" style="vertical-align:bottom;" | {| class="wikitable" style="vertical-align:bottom;" | ||
|- | |- | ||
+ | ! | ||
+ | ! mW/cm^2 | ||
+ | ! % of output | ||
+ | |- | ||
| NO MASK | | NO MASK | ||
− | | | + | | ~10 |
− | | 100% | + | | 100% |
|- | |- | ||
| GLASS MASK | | GLASS MASK | ||
− | | | + | | ~9 |
| 87.5% | | 87.5% | ||
|- | |- | ||
| GLASS + FILM MASK | | GLASS + FILM MASK | ||
− | | | + | | ~7 |
| 68.5% | | 68.5% | ||
|- | |- | ||
| GLASS + LP FILTER | | GLASS + LP FILTER | ||
− | | | + | | ~5 |
− | | 47 | + | | 47% |
|- | |- | ||
| GLASS + FILM + LP FILTER | | GLASS + FILM + LP FILTER | ||
− | | | + | | ~4 |
− | | 37 | + | | 37% |
|} | |} | ||
Line 61: | Line 65: | ||
* [https://nemo.nano.upenn.edu/media/tool_documents/ma-03-abm-mask-aligner/MA-03_SOP_v01.pdf SOP] | * [https://nemo.nano.upenn.edu/media/tool_documents/ma-03-abm-mask-aligner/MA-03_SOP_v01.pdf SOP] | ||
* [https://www.youtube.com/watch?v=cRzLljt0VLs Video - Standard procedure for previous model] *good overview, note slight differences* | * [https://www.youtube.com/watch?v=cRzLljt0VLs Video - Standard procedure for previous model] *good overview, note slight differences* | ||
− | * [https://www.youtube.com/watch?v=Q1DvZBQgKhI&list=PLiihbHV9HgpX_9m5Khz2wn-XaxM5-yErU&index=16 Video - | + | * [https://www.youtube.com/watch?v=Q1DvZBQgKhI&list=PLiihbHV9HgpX_9m5Khz2wn-XaxM5-yErU&index=16 Video - Alignment Marks ] |
Latest revision as of 11:52, 29 April 2025
Tool Name | ABM Mask Aligner |
---|---|
Instrument Type | Lithography |
Staff Manager | Ana Cohen |
Lab Location | Bay 6 |
Tool Manufacturer | ABM |
Tool Model | |
NEMO Designation | MA-03 |
Lab Phone | xxxxx |
SOP Link | SOP |
Description
The ABM Mask Aligner is a manual and versatile mask aligner with top-side alignment and substrate capabilities from 100mm down to small pieces. Requires a 5" mask or 5" glass plate with film mask.
Applications
Tool is used primarily for SU8 exposure. It can also be used for aligning PDMS components for PDMS-to-PDMS bonding.
Exposure time = dose (mJ/cm^2) / intensity (mW/cm^2) Dose can be determined from the resist data sheet. See table below for intensities.
To obtain vertical sidewalls with a Cr glass mask, use the long pass filter (PL-360-LP) which eliminates UV emission below 350nm. Do not use with film masks. Inherent defects in film masks will be accentuated, resulting in worse results.
mW/cm^2 | % of output | |
---|---|---|
NO MASK | ~10 | 100% |
GLASS MASK | ~9 | 87.5% |
GLASS + FILM MASK | ~7 | 68.5% |
GLASS + LP FILTER | ~5 | 47% |
GLASS + FILM + LP FILTER | ~4 | 37% |
More information about Soft Lithography processing can be found under Process Resources
Resources
MA-01 to MA-03 Calculator
SOPs & Troubleshooting
- SOP
- Video - Standard procedure for previous model *good overview, note slight differences*
- Video - Alignment Marks