(Created page with "The QNF provides a variety of standard resists to meet demands for most applications. Some specialty resists are also sold through the QNF Stockroom. A summary of stocked resi...") |
|||
Line 1: | Line 1: | ||
The QNF provides a variety of standard resists to meet demands for most applications. Some specialty resists are also sold through the QNF Stockroom. A summary of stocked resists along with some processing information can be found in the table below. Other similar options that may be available in QNF are also listed. | The QNF provides a variety of standard resists to meet demands for most applications. Some specialty resists are also sold through the QNF Stockroom. A summary of stocked resists along with some processing information can be found in the table below. Other similar options that may be available in QNF are also listed. | ||
− | == QNF Supplied Standard Photoresists == | + | === QNF Supplied Standard Photoresists === |
{| class="wikitable sortable" | {| class="wikitable sortable" | ||
! Resist !! Tone !! Notes !! Alternatives !! Datasheet | ! Resist !! Tone !! Notes !! Alternatives !! Datasheet |
Revision as of 14:55, 10 May 2023
The QNF provides a variety of standard resists to meet demands for most applications. Some specialty resists are also sold through the QNF Stockroom. A summary of stocked resists along with some processing information can be found in the table below. Other similar options that may be available in QNF are also listed.
QNF Supplied Standard Photoresists
Resist | Tone | Notes | Alternatives | Datasheet |
---|---|---|---|---|
S1805 | + | General | KL5305 | Datasheet |
S1813 | + | General | KL5315 | Datasheet |
S1818 | + | General | Datasheet | |
SPR 220-3 | + | Etch | KPRO-3, KL6003, AZ3330F | Datasheet |
SPR 220-4.5 | + | Etch | KPRO-3, KL6003, AZ3330F | Datasheet |
SPR 220-7 | + | Etch | AZ 12XT, AZ P4620 | Datasheet |
AZ 3330F | + | General, Metal RIE, Plating | SPR 220-3, SPR 220-4.5, K-PRO 3, KL60003 | Datasheet |
NR7-3000P | - | Etch, General | Datasheet | |
APOL-LO 3202 | - | Liftoff | Datasheet | |
IP-Dip | - | Nanoscribe | ||
HARE SQ 2 | - | Epoxy | SU-8 2005 | Datasheet |
HARE SQ 50 | - | Epoxy | SU-8 2050 | Datasheet |