Difference between revisions of "Resists at QNF"
Jump to navigation
Jump to search
Line 71: | Line 71: | ||
|- | |- | ||
| H-SiQ 6%|| - || HSQ Equivalent || || [https://upenn.box.com/s/bv53alommdr2en6s6byrlm4psxdjohzp Datasheet] | | H-SiQ 6%|| - || HSQ Equivalent || || [https://upenn.box.com/s/bv53alommdr2en6s6byrlm4psxdjohzp Datasheet] | ||
+ | |} | ||
+ | |||
+ | === Other Resists === | ||
+ | {| class="wikitable sortable" | ||
+ | ! Resist !! Tone !! Notes !! Alternatives !! Datasheet | ||
+ | |- | ||
+ | | LOR 3A|| N/A || Liftoff, Non-imaging || || [https://upenn.box.com/s/ugfgv8xix7vda56ddaodqv3za44m6syk Datasheet] | ||
+ | |- | ||
+ | | PMGI SF 5S|| N/A || Liftoff, Non-imaging || || [https://upenn.box.com/s/ugfgv8xix7vda56ddaodqv3za44m6syk Datasheet] | ||
+ | |- | ||
+ | | PMGI SF 2S|| N/A || Liftoff, Non-imaging || || [https://upenn.box.com/s/ugfgv8xix7vda56ddaodqv3za44m6syk Datasheet] | ||
+ | |- | ||
+ | | NXR-1025|| N/A || Stockroom, Nanoimprint resist || || [https://upenn.box.com/s/wmal2jasuw6m9nqjykz6p8i2ijdn61fm Datasheet] | ||
+ | |} | ||
+ | |||
+ | === Miscellaneous === | ||
+ | These may be available but are not guaranteed to be stocked | ||
+ | |||
+ | {| class="wikitable sortable" | ||
+ | ! Resist !! Tone !! Notes !! Alternatives !! Datasheet | ||
+ | |- | ||
+ | | KL5305 || + || General || S1805 || [https://upenn.box.com/s/1ixn9uek8d78y16x3auicmso433glmvv Datasheet] | ||
+ | |- | ||
+ | | KL5315 || + || General || S1813 || [https://upenn.box.com/s/1ixn9uek8d78y16x3auicmso433glmvv Datasheet] | ||
+ | |- | ||
+ | | KL6003 || + || || SPR 220-3, SPR 220-4.5 || [https://upenn.box.com/s/qv98tqy0ark0l7ppmvphdicgs7udst1f Datasheet] | ||
+ | |- | ||
+ | | K-PRO 3 || + || Plating, Etching|| SPR 220-3, SPR 220-4.5|| [https://upenn.box.com/s/v0hwe0p0u3la1oodz3g45qjw0yl54z7f Datasheet] | ||
+ | |- | ||
+ | | AZ 12XT-20PL-15 || + || Thick Resist, Plating, Packaging || SPR 220-7, AZ P4620 || [https://upenn.box.com/s/dj5l9rrsg0k8g8opdegrylhkgypev9w9 Datasheet] | ||
+ | |- | ||
+ | | AZ P4620|| + || Thick Resist, Plating, Packaging || SPR 220-7, AZ 12XT-20PL-15 || [https://upenn.box.com/s/0r8meepoyq0b1jux7ubudcpt70clau48 Datasheet] | ||
+ | |- | ||
+ | | ma-N 2403|| - || e-beam/DUV Mix and Match || || [https://upenn.box.com/s/7ywdt8x3fqda3p21l4es7fyd98s0fbep Datasheet] | ||
|} | |} |
Revision as of 12:05, 11 May 2023
The QNF provides a variety of standard resists to meet demands for most applications. Some specialty resists are also sold through the QNF Stockroom. A summary of stocked resists along with some processing information can be found in the table below. Other similar options that may be available in QNF are also listed.
QNF Supplied Standard Photoresists
Resist | Tone | Notes | Alternatives | Datasheet |
---|---|---|---|---|
S1805 | + | General | KL5305 | Datasheet |
S1813 | + | General | KL5315 | Datasheet |
S1818 | + | General | Datasheet | |
SPR 220-3 | + | Etch | KPRO-3, KL6003, AZ3330F | Datasheet |
SPR 220-4.5 | + | Etch | KPRO-3, KL6003, AZ3330F | Datasheet |
SPR 220-7 | + | Etch | AZ 12XT, AZ P4620 | Datasheet |
AZ 3330F | + | General, Metal RIE, Plating | SPR 220-3, SPR 220-4.5, K-PRO 3, KL6003 | Datasheet |
NR7-3000P | - | Etch, General | Datasheet | |
APOL-LO 3202 | - | Liftoff | Datasheet | |
IP-Dip | - | Nanoscribe | ||
HARE SQ 2 | - | Epoxy | SU-8 2005 | Datasheet |
HARE SQ 50 | - | Epoxy | SU-8 2050 | Datasheet |
Stockroom Photoresists
Resist | Tone | Notes | Alternatives | Datasheet |
---|---|---|---|---|
SU-8 2005 | - | Epoxy | HARE SQ 2 | Datasheet |
SU-8 2050 | - | Epoxy | HARE SQ 50 | Datasheet |
SU-8 2100 | - | Epoxy | HARE SQ 50 | Datasheet |
SU-8 3050 | - | Epoxy | HARE SQ 50 | Datasheet |
Standard e-beam Resists
Resist | Tone | Notes | Alternatives | Datasheet |
---|---|---|---|---|
495 PMMA A8 | + | Lower Resolution | Datasheet | |
495 PMMA A4 | + | Lower Resolution | Datasheet | |
495 PMMA A2 | + | Lower Resolution | Datasheet | |
950 PMMA A4 | + | High Resolution | Datasheet | |
950 PMMA A2 | + | High Resolution | 1000 HARP 0.1 | Datasheet |
1000 HARP 1.3 | + | High Resolution | Datasheet | |
1000 HARP 0.1 | + | High Resolution | 950 PMMA A2 | Datasheet |
Stockroom e-beam Resists
Resist | Tone | Notes | Alternatives | Datasheet |
---|---|---|---|---|
ZEP 520A | + | Thicker formulation | Datasheet | |
ZEP 520A-7 | + | Thinner formulation | Datasheet | |
H-SiQ 6% | - | HSQ Equivalent | Datasheet |
Other Resists
Resist | Tone | Notes | Alternatives | Datasheet |
---|---|---|---|---|
LOR 3A | N/A | Liftoff, Non-imaging | Datasheet | |
PMGI SF 5S | N/A | Liftoff, Non-imaging | Datasheet | |
PMGI SF 2S | N/A | Liftoff, Non-imaging | Datasheet | |
NXR-1025 | N/A | Stockroom, Nanoimprint resist | Datasheet |
Miscellaneous
These may be available but are not guaranteed to be stocked
Resist | Tone | Notes | Alternatives | Datasheet |
---|---|---|---|---|
KL5305 | + | General | S1805 | Datasheet |
KL5315 | + | General | S1813 | Datasheet |
KL6003 | + | SPR 220-3, SPR 220-4.5 | Datasheet | |
K-PRO 3 | + | Plating, Etching | SPR 220-3, SPR 220-4.5 | Datasheet |
AZ 12XT-20PL-15 | + | Thick Resist, Plating, Packaging | SPR 220-7, AZ P4620 | Datasheet |
AZ P4620 | + | Thick Resist, Plating, Packaging | SPR 220-7, AZ 12XT-20PL-15 | Datasheet |
ma-N 2403 | - | e-beam/DUV Mix and Match | Datasheet |