+ | == Processes == | ||
+ | The following exposure parameters may be used to direct write into S1800 resist (soft baked at 115C for 1 minute) with the 10mm write head. For the optimum focus, please refer to the "AZ1500.txt" or "IP3500.txt" files for the optimum value to use. | ||
+ | |||
Revision as of 16:55, 23 December 2022
Tool Name | Heidelberg DWL 66+ Laser Writer |
---|---|
Instrument Type | Lithography |
Staff Manager | David Jones |
Lab Location | Bay 2 |
Tool Manufacturer | Heidelberg |
Tool Model | DWL 66+ |
NEMO Designation | {{{NEMO_Designation}}} |
Lab Phone | 8-9799 |
SOP Link | SOP |
Description
The fully automated DWL 66+ laser writing system is located inside an environment chamber for stable environment of the system with controlled laminar airflow and temperature stability. The chamber is situated on a granite base with air cushions for vibration isolation. The optical system includes highly reflective mirrors and acousto-optic modulators for real-time beam correction.
Lens & Resolution
- 2 mm lens (optical autofocus): 600 nm
- 10 mm lens (pneumatic autofocus): 2 µm
- 40 mm lens (pneumatic autofocus): 10 µm
Applications
- Patterning of photomasks
- Direct laser writing of patterns
Processes
The following exposure parameters may be used to direct write into S1800 resist (soft baked at 115C for 1 minute) with the 10mm write head. For the optimum focus, please refer to the "AZ1500.txt" or "IP3500.txt" files for the optimum value to use.