The Filmetrics F40 is a microscope-mounted thin-film measurement system, allowing you to non-destructively measure thin-film thicknesses in small (patterned) areas on your sample. The Filmetrics software then performs curve-fitting to determine the thickness and/or refractive index of the measured films.


Applications
  • Thin-film thickness optical measurements