Difference between revisions of "What is Chemical Vapor Deposition (CVD)?"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
 
(3 intermediate revisions by the same user not shown)
Line 3: Line 3:
 
The basic process involves the following steps:
 
The basic process involves the following steps:
  
# '''Precursor Delivery:''' Precursor gases (or vapors) are introduced into a reaction chamber containing the substrate material.
+
#'''Precursor Delivery:''' Precursor gases (or vapors) are introduced into a reaction chamber containing the substrate material.
# '''Chemical Reaction:''' The precursor molecules react with the substrate surface or with other reactive species present in the chamber, leading to the deposition of a thin film of material on the substrate.
+
#'''Chemical Reaction:''' The precursor molecules react with the substrate surface or with other reactive species present in the chamber, leading to the deposition of a thin film of material on the substrate.
# '''Film Growth:''' The deposited material grows on the substrate surface as the chemical reaction continues. The growth rate can be controlled by adjusting parameters such as precursor flow rate, temperature, and pressure.
+
#'''Film Growth:''' The deposited material grows on the substrate surface as the chemical reaction continues. The growth rate can be controlled by adjusting parameters such as precursor flow rate, temperature, and pressure.
# '''Evacuation:''' Any unreacted precursor gases, reaction byproducts, and excess materials are removed from the chamber through evacuation or purging.
+
#'''Evacuation:''' Any unreacted precursor gases, reaction byproducts, and excess materials are removed from the chamber through evacuation or purging.
  
 
CVD offers a wide range of materials growth possibilities and provides:
 
CVD offers a wide range of materials growth possibilities and provides:
Line 12: Line 12:
 
* Scalability for large-area deposition.
 
* Scalability for large-area deposition.
 
* Compatibility with various substrate materials.
 
* Compatibility with various substrate materials.
 +
 +
Click on the link below for an excellent introductory CVD video on YouTube.
 +
 +
* [https://www.youtube.com/watch?v=pZuhK3jsMMY| Chemical Vapor Deposition]

Latest revision as of 12:14, 9 April 2024

Chemical Vapor Deposition (CVD) is a thin-film deposition technique in which thin films are deposited onto a substrate surface through the chemical reaction of vapor-phase precursor molecules.

The basic process involves the following steps:

  1. Precursor Delivery: Precursor gases (or vapors) are introduced into a reaction chamber containing the substrate material.
  2. Chemical Reaction: The precursor molecules react with the substrate surface or with other reactive species present in the chamber, leading to the deposition of a thin film of material on the substrate.
  3. Film Growth: The deposited material grows on the substrate surface as the chemical reaction continues. The growth rate can be controlled by adjusting parameters such as precursor flow rate, temperature, and pressure.
  4. Evacuation: Any unreacted precursor gases, reaction byproducts, and excess materials are removed from the chamber through evacuation or purging.

CVD offers a wide range of materials growth possibilities and provides:

  • Excellent film uniformity and conformity.
  • Scalability for large-area deposition.
  • Compatibility with various substrate materials.