File:SiN etch on DE-04.png
Jump to navigation
Jump to search
Size of this preview: 747 × 600 pixels. Other resolutions: 299 × 240 pixels | 1,798 × 1,444 pixels.
Original file (1,798 × 1,444 pixels, file size: 2.12 MB, MIME type: image/png)
Summary
SiN etch on DE04 CHF3O2
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 13:44, 16 September 2024 | 1,798 × 1,444 (2.12 MB) | Azadi (talk | contribs) | ||
| 13:38, 16 September 2024 | 2,876 × 1,618 (2.59 MB) | Azadi (talk | contribs) | SiN etch on DE04 CHF3O2 |
You cannot overwrite this file.
File usage
The following page uses this file: