Difference between revisions of "Oxford Cobra ICP Etcher"

From Quattrone Nanofabrication Facility
Jump to navigation Jump to search
(update to NEMO)
 
(6 intermediate revisions by 2 users not shown)
Line 7: Line 7:
 
| imagecaption =  
 
| imagecaption =  
 
| Instrument_Type = Etch
 
| Instrument_Type = Etch
| Staff_Manager = Sam Azadi
+
| Staff_Manager = [[Sam Azadi | Sam Azadi]]
 
| Lab_Location = Bay 2
 
| Lab_Location = Bay 2
 
| Tool_Manufacturer = Oxford Instruments
 
| Tool_Manufacturer = Oxford Instruments
 
| Tool_Model = Cobra PlasmaPro 100
 
| Tool_Model = Cobra PlasmaPro 100
| Iris_Designation = DE-05
+
| NEMO_Designation = DE-05
 
| Lab_Phone = 215-898-9748
 
| Lab_Phone = 215-898-9748
 
| SOP Link = [https://repository.upenn.edu/scn_sop/19/ SOP]
 
| SOP Link = [https://repository.upenn.edu/scn_sop/19/ SOP]
Line 17: Line 17:
  
 
== Description ==
 
== Description ==
Oxford PlasmaPro 100 is an inductively coupled plasma (ICP) etcher. The tool uses an RF magnetic field to induce an RF electric field and energize the electrons that result in the ionization of gas molecules and atoms at low pressures. The plasma created in the ICP tool is denser, which allows for a wider range of etching.
+
Oxford PlasmaPro 100 is an inductively coupled plasma (ICP) etcher. The tool uses an RF magnetic field to induce an RF electric field and energize the electrons that result in the ionization of gas molecules and atoms at low pressures.
 +
* Max ICP power: 3 kW
 +
* Max RF power: 200 W
  
 
The tool is connected to the following gases:
 
The tool is connected to the following gases:
Line 29: Line 31:
 
* Etch of Al, Cr, Ti, Nb, hafnia, alumina ....
 
* Etch of Al, Cr, Ti, Nb, hafnia, alumina ....
 
- for a complete list of materials etched in the tool please refer to the SOP at the bottom off this page
 
- for a complete list of materials etched in the tool please refer to the SOP at the bottom off this page
 +
 +
NOTE: Au and Ag, Se, and Li compounds are NOT ALLOWED in the system
  
 
== Resources ==
 
== Resources ==

Latest revision as of 13:08, 3 January 2024


Oxford Cobra ICP Etcher
DE-05.jpeg
Tool Name Oxford Cobra ICP Etcher
Instrument Type Etch
Staff Manager Sam Azadi
Lab Location Bay 2
Tool Manufacturer Oxford Instruments
Tool Model Cobra PlasmaPro 100
NEMO Designation DE-05
Lab Phone 215-898-9748
SOP Link SOP

Description

Oxford PlasmaPro 100 is an inductively coupled plasma (ICP) etcher. The tool uses an RF magnetic field to induce an RF electric field and energize the electrons that result in the ionization of gas molecules and atoms at low pressures.

  • Max ICP power: 3 kW
  • Max RF power: 200 W

The tool is connected to the following gases: BCl3, Cl2, Ar, O2, SF6, CF4, and CHF3.

Applications
  • Etch of Si
  • Etch of SiO2
  • Etch of SiNx
  • Etch of InP
  • Etch of Al, Cr, Ti, Nb, hafnia, alumina ....

- for a complete list of materials etched in the tool please refer to the SOP at the bottom off this page

NOTE: Au and Ag, Se, and Li compounds are NOT ALLOWED in the system

Resources

SOPs & Troubleshooting